lining: simple and fast method, most basic bricks adopt dry lining method. Adopting this method, a rubber hammer must be used to strike on the large surface, at least three times. 2)Wet Lining requirements: • The mortar on the axial brick joint can help smooth out the irregularity of the surface of the brick and make the stress evenly distributed on the whole brick surface. • Therefore, it is recommended to use mortar wet lining in areas with unstable mechanical or large ovality (such as wheel belt area, large ring gear area, kiln mouth area, deformation area, bell mouth). • The thickness of the mortar in the brick joints during wet lining shall not over than 1 mm, and shall be uniform, and the fullness shall only reach 95% be qualified. • It is strictly forbidden to put excess mortar on the cutter against the small head of the refractory brick